| Patent | Title | Area | Cited by | Status |
|---|---|---|---|---|
| US9702024B2 | Method for the hydrometallurgical recovery of lithium, nickel and cobalt from the lithium transition metal oxide-containing fraction of used galvanic cells | Emerging Cross-Sectional Technologies | 8 | Active |
| US9677153B2 | Method for the hydrometallurgical recovery of lithium from the fraction of used galvanic cells containing lithium, iron and phosphate | Emerging Cross-Sectional Technologies | 2 | Active |
| US11155895B2 | Method for obtaining cesium from aqueous starting solutions | Chemistry; Metallurgy | 0 | Active |
| US10711326B2 | Method for the hydrometallurgical recovery of lithium from the lithium manganese oxide-containing fraction of used galvanic cells | Emerging Cross-Sectional Technologies | 0 | Active |