Propylene polymer for high-tenacity fibers and nonwovens
US10023663B2 · kind B2 · utility
0Cited by
1References
17Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jun 27, 2013 |
| Grant date | Jul 17, 2018 |
| Priority date | — |
| Expiry date | Jun 25, 2035 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T442/60
- WIPO fieldTextile and paper machines
- WIPO sectorMechanical engineering
Abstract
Propylene polymers having a melt flow index in the range from 3.0 dg/min to 8.0 dg/min can be particularly suited for high-tenacity fibers and yarns and nonwovens. The propylene polymers can be produced by a process that includes polymerizing propylene or propylene and at least one comonomer in presence of a Ziegler-Natta polymerization catalyst, an aluminium alkyl, and hydrogen.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.