Reinforced flame retardant polycarbonate composition and molded article comprising same
US10030139B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jul 17, 2017 |
| Grant date | Jul 24, 2018 |
| Priority date | — |
| Expiry date | Jul 17, 2037 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L2205/06
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A polymer composition includes: about 20 wt % to about 80 wt % of a polycarbonate polymer; about 1 wt % to about 20 wt % of a polycarbonate-siloxane copolymer; about 15 wt % to about 35 wt % of a reinforcing filler having a tensile modulus of at least about 150 GPa; and about 4 wt % to about 20 wt % of a flame retardant comprising phosphorous. The polymer composition demonstrates a flexural modulus in an amount equal to or greater than about 10 GPa. Methods of forming a polymer composition and blended thermoplastic compositions are also described.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.