Method of forming a continuous filament spun-laid web
US10030322B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jul 15, 2014 |
| Grant date | Jul 24, 2018 |
| Priority date | — |
| Expiry date | Nov 10, 2036 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T442/681
- WIPO fieldTextile and paper machines
- WIPO sectorMechanical engineering
Abstract
A continuous filament spun-laid web includes a plurality of polymer fibers within the web, the web having a first thickness and the web being free of any thermal or mechanical bonding treatment. Activation of the web results in at least one of an increase from the first thickness prior to activation to a second thickness post activation in which the second thickness is at least about two times greater than the first thickness, a decrease in density of the web post activation in relation to a density of the web prior to activation, the web being configured to withstand an elastic elongation from about 10% to about 350% in at least one of a machine direction (MD) of the web and a cross-direction (CD) of the web, and the web having a tensile strength from about 50 gram-force/cm2 to about 5000 gram-force/cm2.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.