Method for recovering inert material and method for producing acrylic acid using inert material recovered by said method
US10035747B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jul 30, 2015 |
| Grant date | Jul 31, 2018 |
| Priority date | — |
| Expiry date | Jul 30, 2035 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P20/584
- WIPO fieldChemical engineering
- WIPO sectorChemistry
Abstract
The present invention provides a method for allowing a used inert material that has been subjected to a reaction once, which is disposed of in the background art, to be used again as well as a brand-new one. A method of recovering an inert material of the present invention is characterized by in the fixed-bed reactor, the inert material is loaded in an inert material layer provided between a first-stage catalyst layer and a second-stage catalyst layer, the first-stage catalyst layer is loaded with a first-stage catalyst for producing acrolein from propylene, and the second-stage catalyst layer is loaded with a second-stage catalyst for producing acrylic acid from acrolein, the method comprising the steps of: extracting the inert material from the fixed-bed reactor; washing the extracted inert material; and screening the washed inert material.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.