Patent · US Active

Method for preparing double-sealed-end glycol ether

US10040739B2 · kind B2 · utility

0Cited by
3References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 22, 2014
Grant dateAug 7, 2018
Priority date
Expiry dateDec 22, 2034

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P20/584
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

Disclosed is a method for preparing a double end capped glycol ether, the method comprising: introducing into a reactor a raw material comprising a glycol monoether and a monohydric alcohol ether, and enabling the raw material to contact and react with an acidic molecular sieve catalyst to generate a double end capped glycol ether, a reaction temperature being 50-300° C., a reaction pressure being 0.1-15 MPa, a WHSV of the glycol monoether in the raw material being 0.01-15.0 h−1 , and a mole ratio of the monohydric alcohol ether to the glycol monoether in the raw material being 1-100:1. The method of the present invention enables a long single-pass lifespan of the catalyst and repeated regeneration, has a high yield and selectivity of a target product, low energy consumption during separation of the product, a high economic value of a by-product, and is flexible in production scale and application.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.