Rotary friction welding
US10052715B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Oct 19, 2016 |
| Grant date | Aug 21, 2018 |
| Priority date | — |
| Expiry date | Dec 14, 2036 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB23K2103/18
- WIPO fieldMachine tools
- WIPO sectorMechanical engineering
Abstract
A method for welding together pieces which form a curved or angled end product using a friction welding process. The method includes: providing first and second pieces which together define the end product geometry, each piece including an end product geometry portion and a sacrificial weld portion, the sacrificial weld portion forming a dog-leg relative to the end product geometry portion and terminating in a planar weld interface surface. The pieces are arranged with their planar weld interface surfaces together at a weld surface interface and the sacrificial weld portions in coaxial alignment. Mechanical friction is applied between the planar weld interface surfaces sufficient to plastically deform the sacrificial weld portions. An axial force is applied along the co-axis of the sacrificial weld portions sufficient to upset the sacrificial weld portions and bring together the end product geometry portions. The sacrificial geometry portions are removed to provide the end product.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.