Steel sheet for soft-nitriding and method for manufacturing the same

US10077489B2 · kind B2 · utility

0Cited by
2References
2Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 27, 2012
Grant dateSep 18, 2018
Priority date
Expiry dateOct 13, 2033

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/009
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A steel sheet for soft-nitriding has a composition containing: C: 0.05% or more to 0.10% or less; Si: 0.5% or less; Mn: 0.7% or more to 1.5% or less; P: 0.05% or less; S: 0.01% or less; Al: 0.01% or more to 0.06% or less; Cr: 0.5% or more to 1.5% or less; Nb: 0.005% or more to 0.025% or less; and N: 0.005% or less, on a mass percent basis, such that C and Nb satisfy 0.10≤Nb/C≤0.30 (where C and Nb are respective contents of the elements (by mass %)), wherein balance comprises Fe and incidental impurities, and a microstructure that is a complex-phase microstructure containing ferrite and pearlite, and the microstructure having a ratio of a microstructure other than the ferrite and the pearlite of 1% or less, and the microstructure having a ratio of polygonal ferrite in the ferrite of less than 50%.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.