Method for manufacturing a polyacrylonitrile-sulfur composite material

US10096834B2 · kind B2 · utility

1Cited by
0References
21Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 3, 2013
Grant dateOct 9, 2018
Priority date
Expiry dateMar 16, 2034

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A method is provided for manufacturing a polyacrylonitrile-sulfur composite material, the polyacrylonitrile-sulfur composite material having an sp2 hybrid proportion, with respect to the total carbon atoms included in the composite material, of greater than or equal to 85% including the method steps: a) reaction of polyacrylonitrile with sulfur at a temperature of greater than or equal to 450° C., in particular greater than or equal to 550° C.; b) immediate purification of the product obtained in method step a); and c) drying the purified product, if necessary. A composite material manufactured in this way may be used in particular in an active material of a cathode of a lithium-ion battery and offers a particularly high rate capacity. In addition, methods are provided for manufacturing an active material for an electrode, a polyacrylonitrile-sulfur composite material and an energy store.