Patent · US Active

Preparation method for rod-shaped molybdenum oxide and preparation method for molybdenum oxide composite

US10130937B2 · kind B2 · utility

1Cited by
0References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 28, 2015
Grant dateNov 20, 2018
Priority date
Expiry dateAug 28, 2035

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2006/80
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

The present specification relates to a preparation method for rod-shaped molybdenum oxide and a preparation method for a molybdenum oxide composite, the preparation method for rod-shaped molybdenum oxide according to the present invention may be carried out under low temperature and pressure conditions, and thus has an advantage in that it is possible to mass produce rod-shaped molybdenum oxide, and the preparation method for a molybdenum oxide composite according to the present invention has an advantage in that the molybdenum oxide composite may be synthesized at a temperature which is equal to or less than the boiling point of ethanol, and the amount of an ethanol solvent used is reduced.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.