Method for joining metal parts

US10131011B2 · kind B2 · utility

0Cited by
13References
24Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 27, 2013
Grant dateNov 20, 2018
Priority date
Expiry dateMay 19, 2034

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/2982
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

A method for joining a first metal part (11) with a second metal part (12), the metal parts (11,12) having a solidus temperature above 1100 QC. The method comprises: applying a melting depressant composition (14) on a surface (15) of the first metal part (11), the melting depressant composition (14) comprising a melting depressant component that comprises at least 25 wt % boron and silicon for decreasing a melting temperature of the first metal part (11); bringing (202) the second metal part (12) into contact with the melting depressant composition (14) at a contact point (16) on said surface (15); heating the first and second metal parts (11,12) to a temperature above 1100 QC; and allowing a melted metal layer (210) of the first metal component (11) to solidify, such that a joint (25) is obtained at the contact point (16). The melting depressant composition and related products are also described.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.