Method of producing Ni-based superalloy

US10131980B2 · kind B2 · utility

0Cited by
1References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 24, 2016
Grant dateNov 20, 2018
Priority date
Expiry dateMar 24, 2036

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of producing a Ni-based superalloy is provided. A hot working material is used and consisting of a specific composition and has a solvus temperature of a γ′ phase of 1050° C. or more. The method includes: performing heating in a temperature of 980° C. to 1050° C. with an upper limit of −30° C. from the solvus temperature of the γ′ phase, for 10 hours or longer; and performing hot working on the material at a working speed of a strain rate of 2.0/second or more in the above temperature range.