Glass laminate construction for optimized breakage performance

US10137667B2 · kind B2 · utility

3Cited by
13References
18Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 31, 2013
Grant dateNov 27, 2018
Priority date
Expiry dateFeb 12, 2035

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/24967
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

A glass laminate includes at least one chemically-strengthened glass sheets with a thickness not exceeding 2.0 mm and a polymer interlayer between the glass sheets. Flaws are created in the surface of one of the glass sheets in order to weaken the glass laminate upon an impact event on a first side of the laminate, while retaining the strength of the laminate upon impact on the opposing second side of the laminate. The opposing side of the glass sheet with the flaws or a surface of the other glass sheet may be strengthened with an acid etch treatment in order to further strengthen the laminate upon impact on the opposing second side of the laminate.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.