Patent · US Active

Strengthened glass and compositions therefor

US10144198B2 · kind B2 · utility

3Cited by
15References
18Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 29, 2015
Grant dateDec 4, 2018
Priority date
Expiry dateApr 7, 2036

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/315
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A glass laminate structure comprising an external glass sheet and an internal glass sheet wherein one or both of the glass sheets comprises SiO2+B2O3+Al2O3≥86.5 mol. %. and R2O—RO—Al2O3<about 5 mol. %. Exemplary glass sheet can comprise between about 69-80 mol. % SiO2, between about 6-12 mol. % Al2O3, between about 2-10 mol. % B2O3, between about 0-5 mol. % ZrO2, Li2O, MgO, ZnO and P2O5, between about 6-15 mol. % Na2O, between about 0-3 mol. % K2O and CaO, and between about 0-2 mol. % SnO2 to provide a mechanically robust and environmentally durable structure.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.