Patent · US Active

Chemically strengthened glass

US10144670B2 · kind B2 · utility

26Cited by
0References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 6, 2017
Grant dateDec 4, 2018
Priority date
Expiry dateNov 6, 2037

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC03C2204/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention relates to a chemically strengthened glass, in which CT1 and CT5 satisfy CT5/CT1≤0.85, the CT1 satisfies CT1>−38.7×ln(t/1000)+48.2 [MPa] and an internal energy density rE satisfies rE≤23.3×t/1000+15 [kJ/m2]. CS is a surface compressive stress value [MPa], σ (x) is a compressive stress value [MPa] at a position x in a depth direction, DOL is a compressive stress depth [μm], and t is a sheet thickness [μm].

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.