An aqueous polymer composition which when in the form of a film shows excellent elongation at break comprising (i) 5 to 30 wt. % of polyurethane where the acid value of the polyurethane is between 3 to 40 mg KOH/g; (ii) 70 to 95 wt. % of vinyl polymer comprising 20 to 90 wt. % of vinyl polymer with Tg<20° C.; 10 to 80 wt. % of vinyl polymer with Tg≥20° C.; where at least one of the vinyl polymers contains acid functional groups with acid value in the range of from 15 and 240 mg KOH/g.