Patent · US Active

High carbon steel wire rod and method for manufacturing same

US10174399B2 · kind B2 · utility

0Cited by
1References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 23, 2014
Grant dateJan 8, 2019
Priority date
Expiry dateApr 25, 2035

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/009
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A steel wire rod includes required amounts of chemical components and a remainder including Fe and impurities; in which the area ratio of pearlite in a cross section perpendicular to a longitudinal direction is 95% or more and a remainder includes a non-pearlite structure which includes one or more of a bainite, a degenerate pearlite, a proeutectoid ferrite and a proeutectoid cementite; the average block size of the pearlite is 15 μm to 35 μm and the area ratio of the pearlite having a block size of 50 μm or more is 20% or less; and the area ratio of a region where a lamellar spacing of the pearlite is 150 nm or less is 20% or less in a region within a depth from a surface of the steel wire rod of 1 mm or less.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.