Patent · US Active

High performance AlSiMgCu casting alloy

US10174409B2 · kind B2 · utility

3Cited by
6References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 26, 2012
Grant dateJan 8, 2019
Priority date
Expiry dateOct 26, 2032

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/043
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

An aluminum casting alloy has 8.5-9.5 wt. % silicon, 0.5-2.0 wt. % copper (Cu), 0.27-0.53 wt. % magnesium (Mg), wherein the aluminum casting alloy includes copper and magnesium such that 4.7≤(Cu+10Mg)≤5.8, and other elements, the balance being aluminum. Selected elements may be added to the base composition to give resistance to degradation of tensile properties due to exposure to heat. The thermal treatment of the alloy is calculated based upon wt. % composition to solutionize unwanted phases having a negative impact on properties and may include a three level ramp-up and soak to a final temperature followed by cold water quenching and artificial aging.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.