Leaching of minerals
US10190193B2 · kind B2 · utility
0Cited by
3References
17Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Oct 21, 2014 |
| Grant date | Jan 29, 2019 |
| Priority date | — |
| Expiry date | May 25, 2035 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P10/20
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method for treating a mineral composition containing iron, arsenic or other Group VA compounds comprises milling the mineral composition to a particle size of P80 of less than 25 μm and leaching the mineral composition in the presence of lime and/or limestone and a soluble alkali complexing agent and in the presence of an oxygen containing gas at a pH in the range of from 3.5 to 6.