Abstract

A method of manufacturing a rare earth magnet includes: preparing a powder by preparing a rapidly-solidified ribbon by liquid solidification, and by crushing the rapidly-solidified ribbon; manufacturing a sintered compact by press-forming the powder; and manufacturing a rare earth magnet by performing hot deformation processing on the sintered compact to impart anisotropy to the sintered compact. In this method, the rapidly-solidified ribbon is a plurality of fine crystal grains. The powder includes a RE-Fe—B main phase and a grain boundary phase of a RE-X alloy present around the main phase. RE represents at least one of Nd and Pr. X represents a metal element. A nitrogen content in the powder is adjusted to be at least 1,000 ppm and less than 3,000 ppm by performing at least one of the preparation of the powder and the manufacturing of the sintered compact in a nitrogen atmosphere.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.