Porous SiO2-xerogel with a characteristic pore size, stable drying precursors thereof and use of same
US10196274B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | Nov 19, 2010 |
| Grant date | Feb 5, 2019 |
| Priority date | — |
| Expiry date | Nov 19, 2030 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01B33/14
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A porous SiO2 xerogel is produced using temporary pore fillers or solid skeletal supports, which are removed by thermal oxidation at the end of the production process (e.g. carbon or organic), by means of a sol-gel-process by subcritical drying of the gel. The SiO2 xerogel includes pores having a pore size from more than 50 nm to less than 1000 nm. The SiO2 xerogel has a density of less than 400 kg/m3, a carbon content of less than 10%, a thermal conductivity at 800° C. below 0.060 W/m*K, a thermal conductivity at 400° C. below 0.040 W/m*K, and a thermal conductivity at 200° C. below 0.030 W/m*K.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.