Slurry for thermal spraying, thermal spray coating, and method for forming thermal spray coating
US10196536B2 · kind B2 · utility
0Cited by
7References
18Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Mar 7, 2014 |
| Grant date | Feb 5, 2019 |
| Priority date | — |
| Expiry date | Mar 7, 2034 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08K2003/2227
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A thermal spray slurry of the present invention contains ceramic particles in a content of 10% by mass or more and 85% by mass or less, and has a viscosity of 3,000 mPa·s or less. The ceramic particles have an average particle size of, for example, 1 nm or more and 5 μm or less. The thermal spray slurry may further contain a dispersant. The thermal spray slurry may further contain a viscosity modifier. The thermal spray slurry may further contain a flocculant.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.