Method for producing a corrosion-resistant steel sheet
US10227671B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Oct 14, 2013 |
| Grant date | Mar 12, 2019 |
| Priority date | — |
| Expiry date | Oct 18, 2035 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P10/25
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method for producing a corrosion-resistant steel sheet made of an unalloyed or low-alloy and cold-rolled steel having a carbon content of less than 0.1 wt %. The method includes the following steps: applying a metal coating to the steel sheet; annealing the coated steel sheet in a recrystallizing manner by heating the coated steel sheet to temperatures in the recrystallization range by electromagnetic induction in an inert-gas atmosphere; and quenching the coated and annealed steel sheet. The metal coating is fused on during the recrystallization annealing.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.