Methods for producing polyaspartic acids in the presence of methanesulfonic acid
US10233286B2 · kind B2 · utility
0Cited by
20References
20Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Sep 8, 2014 |
| Grant date | Mar 19, 2019 |
| Priority date | — |
| Expiry date | Sep 8, 2034 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02W10/37
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The present invention relates to methods for producing polyaspartic acids with a weight-average molecular weight (Mw) of from 6,000 to 15,000 g/mol. The invention also relates to polyaspartic acids which can be obtained by the method according to the invention, to a composition containing the polyaspartic acids, and to the use thereof as scale inhibitors, dispersants and as an additive in dishwashing agents, detergents or cleaning agents.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.