Anti-corrosion composition comprising at least one first compound and at least one second compound

US10240069B2 · kind B2 · utility

0Cited by
0References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 15, 2016
Grant dateMar 26, 2019
Priority date
Expiry dateNov 15, 2036

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC09J2423/00
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

An anti-corrosion composition includes a first compound including: a first polyisobutylene having an average relative molar mass ranging from about 30,000 to about 100,000 g/mole and a Staudinger index ranging from about 15-70 cm3/g, a first depolymerized butyl rubber with Brookfield viscosity at 66° C. ranging from about 400,000-2,000,000 mPa·s and an average molecular weight ranging from about 20,000-60,000, and combinations thereof. A second compound includes a second polyisobutylene having an average relative molar mass ranging from about 900,000-6,500,000 g/mole and a Staudinger index ranging from about 240-900 cm3/g, at least one second partly cross-linked butyl rubber with a Mooney viscosity at 127° C. ranging from about 65-100 MU. The anti-corrosion composition includes at least one first or at least one second polyisobutylene as well as at least one first or at least one second butyl rubber.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.