Patent · US Active

Nonaqueous electrolyte secondary battery

US10243196B2 · kind B2 · utility

1Cited by
0References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 2, 2015
Grant dateMar 26, 2019
Priority date
Expiry dateDec 23, 2035

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A positive electrode mixture layer (12) includes a first layer (12a) that has a main surface MS and a second layer (12b) formed closer to the positive electrode current collector (11) side than the first layer (12a). A ratio of the volume of the first layer (12a) to the volume of the positive electrode mixture layer (12) is 20 to 75 vol %. The first layer (12a) contains lithium iron phosphate (LFP) (1) and lithium nickel cobalt manganese composite oxide (NCM) (2). A ratio of the mass of the LFP (1) to the total mass of the LFP (1) and the NCM (2) in the first layer (12a) is more than 0 and 80 mass % or less. The second layer (12b) contains NCM (2). A ratio of the mass of the LFP (1) to the total mass of the positive electrode active material in the positive electrode mixture layer (12) is 7.5 to 20 mass %. A maximum pore size of the first layer (12a) is 0.50 to 0.70 μm.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.