Abstract
Provided is a method of recovering rare-earth elements by performing slight pH adjustment of a leachate, which does not require such significant pH adjustment as in conventional methods, reduces cost and effort, and can efficiently recover rare-earth elements in a bauxite residue in a good yield. The method of recovering rare-earth elements is a method of recovering rare-earth elements, the method including: a leaching step of bringing a raw material bauxite residue, which is produced as a by-product in a Bayer process, into contact with a liquid leaching agent to recover a leachate containing rare-earth elements; an extraction step of bringing the leachate into contact with an extraction treatment liquid containing a phosphoric acid ester-based extractant to recover an extract liquid containing the rare-earth elements; and a back extraction step of bringing the extract liquid into contact with a back extraction treatment liquid to recover the rare-earth elements, the leaching step including recovering a leachate having a pH of 0.5 or more and 1.2 or less by using an acidic liquid leaching agent, the extraction step including adjusting the pH of the leachate to 1.0 or more and 1.7 …
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.