Patent · US Active

Method for preparing noble metal hydrogenation catalyst, noble metal hydrogenation catalyst and use thereof

US10252255B2 · kind B2 · utility

0Cited by
8References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 9, 2015
Grant dateApr 9, 2019
Priority date
Expiry dateSep 1, 2037

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC10N2070/00
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

Disclosed are a method for preparing a noble metal hydrogenation catalyst comprising preparing a carrier from a molecular sieve having a 10-member ring structure and/or an amorphous porous material; preparing a noble metal impregnation solution; and preparing noble metal impregnation solutions in a concentration gradient ranging from 0.05 to 5.0 wt % with deionized water, and sequentially impregnating the carrier with the impregnation solutions from low to high concentrations during the carrier impregnation process, or preparing a noble metal impregnation solution at a low concentration ranging from 0.05 to 0.5 wt % and impregnating the carrier by gradually increasing the concentration of the noble metal impregnation solution to 2.0 to 5.0 wt % in the impregnation process, followed by homogenization, drying, and calcination, as well as a noble metal hydrogenation catalyst, use thereof, and a method for preparing lubricant base oil.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.