Abstract
A high temperature, high strength Ni—Co—Cr alloy is provided. The alloy includes, in weight percent (wt. %): 23.5 to 25.5% Cr, 15.0 to 22.0% Co, 1.1 to 2.0% Al, 1.0 to 1.8% Ti, 0.95 to 2.2% Nb, less than 1.0% Mo, less than 1.0% Mn, up to 0.24% Si, less than 3.0% Fe, less than 0.3% Ta, less than 0.3% W, 0.005 to 0.08% C, 0.01 to 0.3% Zr, 0.0008 to 0.006% B, up to 0.05% rare earth metals, and a balance of Ni plus trace impurities.