Abstract
Cement slurries, cured cements, and methods of making cured cement and methods of using cement slurries are provided. The cement slurry contains water, a cement precursor material, an alcohol surfactant having from 10 to 20 carbon atoms and a carboxylic acid comprising an aliphatic chain having from 16 to 18 carbons. In some embodiments, the alcohol surfactant may comprise the formula R—(OC2H4)x—OH where R is a hydrocarbyl group having from 10 to 20 carbons and x is an integer from 1 to 10. The cured cement contains water, cement, an alcohol surfactant having from 10 to 20 carbon atoms and a carboxylic acid comprising an aliphatic chain having from 16 to 18 carbons. In some embodiments, the alcohol surfactant may comprise the formula R—(OC2H4)x—OH where R is a hydrocarbyl group having from 10 to 20 carbons and x is an integer from 1 to 10.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.