Patent · US Active

Process for the preparation of SiOx having a nanoscale filament structure and use thereof as anode material in lithium-ion batteries

US10329157B2 · kind B2 · utility

0Cited by
4References
22Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 28, 2014
Grant dateJun 25, 2019
Priority date
Expiry dateNov 28, 2034

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A process for the preparation of nanofilament particles of SiOx in which x is between 0.8 and 1.2, the process comprising: a step consisting of a fusion reaction between silica (SiO2) and silicon (Si), at a temperature of at least about 1410° C., to produce gaseous silicon monoxide (SiO); and a step consisting of condensation of the gaseous SiO to produce the SiOx nanofilament particles. The process may also comprising using carbon.