Patent · US Active

Silicon-silicon oxide-lithium composite material having nano silicon particles embedded in a silicon:silicon lithium silicate composite matrix, and a process for manufacture thereof

US10333141B2 · kind B2 · utility

0Cited by
1References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 29, 2017
Grant dateJun 25, 2019
Priority date
Expiry dateJun 29, 2037

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A process for producing a silicon:silicon oxide:lithium composite (SSLC) material useful as a negative electrode active material for non-aqueous battery cells includes: producing a partially lithiated SSLC material by way of mechanical mixing; subsequently producing a further prelithiated SSLC material by way of spontaneous lithiation procedure; and subsequently producing a delithiated SSLC material by way of reacting lithium silicide within the dispersed prelithiated SSLC material with organic solvent(s) to extract lithium from the prelithiated SSLC material, until reactivity of lithium silicide within the prelithiated SSLC material with the organic solvent(s) ceases. The delithiated SSLC material is a porous plastically deformable matrix having nano silicon embedded therein. The delithiated SSLC material can have a lithium silicide content of less than 0.5% by weight. A battery cell having as its negative electrode active material an SSLC material as set forth herein can exhibit an irreversible capacity loss of less than 10%.