Patent · US Active

Processes for producing LiMXO4 and products thereof

US10377632B2 · kind B2 · utility

0Cited by
2References
17Claims
0Family size

Assignees

Inventors

Key dates

Filing dateMay 26, 2015
Grant dateAug 13, 2019
Priority date
Expiry dateMay 11, 2036

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

There is provided a process for producing LiMXO4, comprising the steps of reacting a source of lithium, a source of M, and a source of X together, in a melted state at a reaction temperature between 900 to 1450 C, in the presence of an excess of (A) a solid-solid reducing couple having an oxygen partial process at equilibrium (pO2) comprised between 10−8 and 10−15 atm at said reaction temperature according to an Ellingham-Richardson diagram for oxides, or (B) one component of the solid-solid reducing couple together with a gas-gas reducing couple having an oxygen partial pressure equilibrium (pO2) between 10−8 and 10−15 atm at said reaction temperature according to an Ellingham-Richardson diagram of oxides, and under thermic equilibrium and thermodynamic equilibrium. There is also provided a LiMXO4 melt-solidified product free from off-composition impurities.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.