Patent · US Active

Method of manufacturing hot-pressed member

US10384254B2 · kind B2 · utility

2Cited by
0References
2Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 2, 2014
Grant dateAug 20, 2019
Priority date
Expiry dateFeb 16, 2035

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of manufacturing a hot-pressed member including heating a coated steel sheet to 850° C. to 950° C., the coated steel sheet including a substrate steel sheet and a coating layer formed on the substrate steel sheet and containing 10% to 25% by mass of Ni and the balance being Zn and incidental impurities, in which the coating weight of the coating layer is 10 to 90 g/m2 per a side; and starting hot press forming when the temperature of the coated steel sheet which has been heated is 650° C. to 800° C.