Abstract

By using, as a raw material, a thick hot-rolled steel sheet having a chemical composition containing, by mass %, C: 0.02% or more and 0.10% or less, Si: 0.05% or more and 0.30% or less, Mn: 0.80% or more and 2.00% or less, and Nb: 0.010% or more and 0.100% or less and satisfying the condition that a carbon equivalent Ceq is 0.25% or more and 0.50% or less, a microstructure including a bainitic ferrite phase and/or a bainite phase, a high strength of 52 ksi or more in terms of yield strength and a high toughness of −45° C. or lower in terms of fracture transition temperature vTrs, and satisfying the condition that the ratio of the average crystal grain size of the coarsest-grain portion to the average crystal grain size of the finest-grain portion is 2.0 or less in every portion in the wall thickness direction is obtained.