Patent · US Active

Method for transforming Al—Cu—Li alloy sheets improving formability and corrosion resistance

US10400313B2 · kind B2 · utility

0Cited by
4References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 7, 2014
Grant dateSep 3, 2019
Priority date
Expiry dateSep 9, 2036

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/057
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for producing a rolled product 0.5 to 10 mm thick made from an aluminum alloy comprising, in particular, copper and lithium, in which, after solution annealing and quenching, a short heat treatment is carried out in which the sheet reaches a temperature of between 145° C. and 175° C. for 0.1 to 45 minutes, the speed of heating being between 3 and 600° C./min. The sheet obtained at the end of the method according to the invention has high corrosion resistance and is capable of being shaped for producing a structural element for an aircraft, in particular an aircraft fuselage skin.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.