R—Fe—B sintered magnet and making method
US10410775B2 · kind B2 · utility
5Cited by
2References
8Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Mar 31, 2016 |
| Grant date | Sep 10, 2019 |
| Priority date | — |
| Expiry date | Nov 18, 2037 |
Classification
- Technology area (CPC H)Electricity
- CPC primaryH01F41/0293
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
The invention provides an R—Fe—B sintered magnet consisting essentially of 12-17 at % of Nd, Pr and R, 0.1-3 at % of M1, 0.05-0.5 at % of M2, 4.8+2*m to 5.9+2*m at % of B, and the balance of Fe, containing R2(Fe,(Co))14B intermetallic compound as a main phase, and having a core/shell structure that the main phase is covered with grain boundary phases. The sintered magnet exhibits a coercivity of at least 10 kOe despite a low or nil content of Dy, Tb and Ho.