Patent · US Active

Laser system and method forming an edge section of a high purity fused silica glass sheet

US10435324B2 · kind B2 · utility

0Cited by
6References
12Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 16, 2017
Grant dateOct 8, 2019
Priority date
Expiry dateNov 22, 2037

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC03B2201/06
  • WIPO fieldOther special machines
  • WIPO sectorMechanical engineering

Abstract

A system and method for making an edge section of a thin, high purity fused silica glass sheet. The method includes a step of directing a laser to melt through the glass sheet with localized heating of a narrow portion of the glass sheet to form an edge section of the glass sheet, and continuing the edge section to form a closed loop defining a perimeter of the glass sheet. The method further includes rapidly cooling the glass sheet through the glass transition temperature as the melted glass of the edge section contracts and/or solidifies to form an unrefined-bullnose shape extending between first and second major surfaces of the glass sheet.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.