Optical fiber for applications requiring high system optical signal-to-noise ratio performance and low degradation from nonlinear impairments
US10451795B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Nov 7, 2018 |
| Grant date | Oct 22, 2019 |
| Priority date | — |
| Expiry date | Nov 7, 2038 |
Classification
- Technology area (CPC G)Physics
- CPC primaryG02B6/02019
- WIPO fieldOptics
- WIPO sectorInstruments
Abstract
A optical fiber having core and cladding regions, a primary coating, and a secondary coating may be defined in part by a curve relating the microbend sensitivity to a ratio of the elastic modulus of the secondary coating to the elastic modulus of the primary coating (as plotted on respective y and x axes). The curve has a substantially peaked shape defined by a positive-slope region and a negative-slope region. The ratio of the elastic modulus of the secondary coating to the elastic modulus of the primary coating is within the positive-slope region.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.