Patent · US Active

High thermal stability melamine octamolybdate and use thereof as a smoke suppressant in polymer compositions

US10465062B2 · kind B2 · utility

1Cited by
9References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 7, 2017
Grant dateNov 5, 2019
Priority date
Expiry dateFeb 23, 2038

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08K2003/2227
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

Processes for producing melamine octamolybdates having high thermal stability include a step of reacting molybdenum trioxide and melamine in an acidic aqueous system at a pH of less than or equal to about 4 to form a slurry of the melamine octamolybdate. The resulting melamine octamolybdate can be characterized by a decomposition onset temperature (or a temperature at a weight loss of 1%, or a temperature at a weight loss of 2%) on a thermogravimetric analysis curve of greater than 300° C., and is useful in polymer compositions as a smoke suppressant.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.