Patent · US Active

Carbon material, method for manufacturing same, and use thereof

US10508038B2 · kind B2 · utility

0Cited by
0References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 16, 2016
Grant dateDec 17, 2019
Priority date
Expiry dateJul 14, 2036

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02T10/70
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

The present provides a carbon material containing 50 to 1,000 ppm by mass of vanadium (V), wherein a mean particle diameter D50 is 3 to 7 μm; a tapping density after 400 times of tapping is 0.40 to 1.00 g/cm3; a BET specific surface area is 4.0 to 12.0 m2/g; an R value (ID/IG) measured in the spectrum observed by Raman spectroscopy is 0.10 to 0.30; and an interplanar spacing d002 of plane (002) (nm) and Lc002 (nm) as being the size in the c-axis direction of the graphite crystals satisfy the relationship represented by the following formulae (1) and (2) 0.3362≤d002≤0.3370  (1)−23660×d002+8010≤Lc002≤−23660×d002+8025  (2); which is suitable for a non-aqueous electrolytic secondary battery having a low resistance and a high coulomb efficiency; a method for producing the same; a carbon material for a battery electrode; an electrode; and a lithium-ion secondary battery using the above-described carbon material.