Transparent hydrophobic mixed oxide coatings and methods
US10519063B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Aug 18, 2017 |
| Grant date | Dec 31, 2019 |
| Priority date | — |
| Expiry date | Mar 30, 2038 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC03C2218/112
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A hydrophobic coating and a method for applying such a coating to a surface of a substrate. The method includes applying a coating composition to the surface and heating the coated surface at a cure temperature from about 300° C. to about 600° C. for a time from about 2 hours to about 48 hours. The coating composition is applied to the surface by an application method selected from the group consisting of flowing, dipping, and spraying. The coating composition comprises a yttrium compound, an additive selected from the group consisting of a cerium compound and a dispersion of yttrium oxide nanoparticles, a water-soluble polymer, and a solvent solution of de-ionized water and a water-soluble alcohol.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.