High Cr-based austenitic stainless steel

US10519533B2 · kind B2 · utility

1Cited by
1References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 3, 2016
Grant dateDec 31, 2019
Priority date
Expiry dateSep 30, 2036

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E20/16
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A high Cr austenitic stainless steel with a chemical composition consisting of in terms of % by mass, 0.03 to 0.12% of C, 0.10 to 1.00% of Si, 0.10 to 3.00% of Mn, 0.030% or less of P, 0.020% or less of S, 21.50 to 28.00% of Cr, more than 26.00 and not more than 35.00% of Ni, more than 2.00 and not more than 5.00% of W, 0.80% or less of Co, 0.01 to 0.70% of V, 0.15 to 1.00% of Nb, 0.001 to 0.040% of Al, 0.0001 to 0.0100% of B, 0.010 to 0.400% of N, 0.001 to 0.200% of Zr, 0.001 to 0.200% of Nd, 0.001 to 0.200% of Ta, 0.020 to 0.200% of Ta+0.8Nd+0.5Zr, 0.025% or less of Ti+Sn+Sb+Pb+As+Bi, 0.0090% or less of O, and a remainder consisting of Fe and impurities.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.