Wrought aluminum alloy

US10557186B2 · kind B2 · utility

0Cited by
1References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 3, 2017
Grant dateFeb 11, 2020
Priority date
Expiry dateMay 8, 2038

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/053
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Provided is a wrought aluminum alloy including 5.5 to 6.0 wt % of Zn, 2.0 to 2.5 wt % of Mg, 0.2 to 0.6 wt % of Cu, 0.1 to 0.2 wt % of Cr, at most 0.2 wt % (and more than 0 wt %) of Fe, at most 0.2 wt % (and more than 0 wt %) of Mn, at most 0.2 wt % (and more than 0 wt %) of Si, at most 0.1 wt % (and more than 0 wt %) of Ti, and at most 0.05 wt % (and more than 0 wt %) of Sr, with the remainder being Al.