Abstract

Alloys, processes for preparing the alloys, and articles including the alloys are provided. The alloys can include, by weight, about 0.01% to about 1% vanadium, 0% to about 0.04% carbon, 0% to about 8% niobium, 0% to about 1% titanium, 0% to about 0.04% boron, 0% to about 1% tungsten, 0% to about 1% tantalum, 0% to about 1% hafnium, and 0% to about 1% ruthenium, the balance essentially molybdenum and incidental elements and impurities.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.