Method for green synthesis of uniform- and large-particle-size polystyrene particles
US10604599B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | May 29, 2018 |
| Grant date | Mar 31, 2020 |
| Priority date | — |
| Expiry date | Oct 30, 2038 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08F2500/24
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A method for green synthesis of uniform- and large-particle-size polystyrene particles, comprising steps of: prepolymerizing styrene at 70□ to 75□ for 1 h to 6 h in advance while stirring, adding divinylbenzene dissolved with initiators to the styrene, and stirring for 10 min to 30 min to obtain oil phase; heating lactic acid or an aqueous solution of lactic acid to 70□ to 80□, adding the oil phase to dispersed phase by a constant-pressure device, maintaining the temperature for 2 h, heating to 80±5□ and then maintaining the temperature for 1 h, and heating to 85±5□ and then maintaining the temperature for 3 h to 6 h, to obtain polystyrene particles with a uniform particle size ranging from 0.7 mm to 2.0 mm.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.