Porous ultra-soft ultra-fine denier polyester fiber and its preparation method

US10604621B2 · kind B2 · utility

0Cited by
1References
9Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 26, 2017
Grant dateMar 31, 2020
Priority date
Expiry dateJun 26, 2037

Classification

  • Technology area (CPC D)Textiles; Paper
  • CPC primaryD10B2331/04
  • WIPO fieldTextile and paper machines
  • WIPO sectorMechanical engineering

Abstract

A porous ultra-soft ultra-fine denier polyester fiber and preparation method. The modified polyester is spun with a porous spinneret to produce the porous ultra-soft ultra-fine denier polyester fiber, and the spinneret holes on the porous spinneret are arranged in an elliptical arrangement. The porous ultra-soft ultra-fine denier polyester fiber is obtained by metering, extruding, cooling, oiling and high-speed winding the modified polyester chips. The preparation method of modified polyester is as follows: terephthalic acid reacts with ethylene glycol to produce ethylene terephthalate. The modified polyester is obtained by the reaction of terephthalic acid with branched diol. The fiber of the invention has good properties and the deviation rate of fiber density. The deviation rate of fiber density is ≤0.5%, the CV value of breaking strength is ≤4.0%, the CV value of elongation at break is ≤8.0%, the CV value of yarn unevenness is ≤2.0%.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.