Patent · US Active

Manufacturing method of wear-resistant iron-based sintered alloy and wear-resistant iron-based sintered alloy

US10619229B2 · kind B2 · utility

1Cited by
1References
3Claims
0Family size

Assignees

Inventors

Key dates

Filing dateSep 13, 2017
Grant dateApr 14, 2020
Priority date
Expiry dateMar 22, 2038

Classification

  • Technology area (CPC F)Mechanical Engineering; Lighting; Heating
  • CPC primaryF01L2303/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

An iron alloy powder consists of, when the entirety thereof is assumed to be 100 mass %, Cr: 2.5 mass % to 3.5 mass %, Mo: 0.4 mass % to 0.6 mass %, and Fe and inevitable impurities as the balance, a mixed powder consisting of 15 mass % to 40 mass % of the iron alloy powder, 1.2 mass % to 1.8 mass % of a copper powder, 0.5 mass % to 1.0 mass % of a graphite powder, and a pure iron powder as the balance when the entire mixed powder is assumed to be 100 mass % is compacted into a compact, and the compact is sintered while transforming a structure derived from the pure iron powder into a structure in which a ferritic structure and a pearlitic structure are mixed and transforming a structure derived from the iron alloy powder into a martensitic structure.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.