Method of preparing positive electrode active material for secondary battery and positive electrode active material for secondary battery prepared thereby
US10637056B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jul 4, 2017 |
| Grant date | Apr 28, 2020 |
| Priority date | — |
| Expiry date | Jul 4, 2037 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/10
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
Provided are a method of preparing a positive electrode active material for a secondary battery, in which the positive electrode active material is uniformly doped with various doping elements without worrying about surface damage of the active material and characteristics degradation by including mixing a metal precursor for a positive electrode active material and a raw material including a doping element, in which an average particle diameter ratio is in a range of 5:1 to 2,000:1, using acoustic resonance to prepare a precursor doped with the doping element, and mixing the doped precursor with a lithium raw material and performing a heat treatment, and a positive electrode active material which has improved structure stability by being prepared by the above method and may improve battery characteristics, for example, capacity reduction may be minimized and cycle characteristics may be improved when used in the battery.