Patent · US Active

Method for increasing the particle size of ammonium octamolybdate (AOM)

US10640652B2 · kind B2 · utility

0Cited by
3References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 24, 2015
Grant dateMay 5, 2020
Priority date
Expiry dateFeb 8, 2036

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2004/62
  • WIPO fieldTextile and paper machines
  • WIPO sectorMechanical engineering

Abstract

Methods of increasing the particle size of ammonium octamolybdate (AOM) pigment powder are provided. A method can include heating the AOM pigment powder to a temperature above 20° C. for a given amount of time. An ink composition can be produced by formulating AOM pigment powder with increased particle size and incorporating the AOM pigment powder into an ink composition.